ISO 9001:2015 Certified | Cage Code: 7L0f6

TYPICAL PROPERTIES of ABS (Acrylonitrile-Butadiene-Styrene)

ASTM or UL test Property ABS
PHYSICAL
D792 Density (lb/in³)(g/cm³) 0.038 1.04
D570 Water Absorption, 24 hrs (%)
MECHANICAL
D638 Tensile Strength (psi) 6,500
D638 Tensile Modulus (psi) 340,000
D638 Tensile Elongation at Break (%) 25
D790 Flexural Strength (psi) 11,000
D790 Flexural Modulus (psi) 320,000
D695 Compressive Strength (psi)
D695 Compressive Modulus (psi)
D785 Hardness, Rockwell R105
D256 IZOD Notched Impact (ft-lb/in) 7.0
THERMAL
D696 Coefficient of Linear Thermal Expansion (x 10-5 in./in./°F) 5.3
D648 Heat Deflection Temp (°F / °C) at 264 psi 215 / 102
D3418 Melting Temp (°F / °C) – / –
Max Operating Temp (°F / °C) 140 / 60
C177 Thermal Conductivity (BTU-in/ft²-hr-°F)
(x 10-4 cal/cm-sec-°C)
– –
UL94 Flammability Rating H-B
ELECTRICAL
D149 Dielectric Strength (V/mil) short time, 1/8″ thick
D150 Dielectric Constant at 60 Hz
D150 Dissipation Factor at 60 Hz
D257 Volume Resistivity (ohm-cm)at 50% RH 1015